The paper summarizes the results of observation and quantitative analysis of porosity in IN713C superalloy in as-cast and after the creep test. The sources of porosity in castings are shortly described and the methodology of pores measurement is circumscribed. The results of pores in as-cast and after the creep test were shown and, finally, the interpretation of the result was presented.
Informacje: Czasopismo Techniczne, 2016, Mechanika Zeszyt 4-M 2016, s. 21 - 26
Typ artykułu: Oryginalny artykuł naukowy
Tytuły:
Metallographic study of porosity in IN713C superalloy in as-cast and after creep test
Metallographic study of porosity in IN713C superalloy in as-cast and after creep test
Institute of Materials Science, Faculty of Materials Science and Metallurgy, Silesian University of Technology
Publikacja: 19.12.2016
Status artykułu: Otwarte
Licencja: Żadna
Udział procentowy autorów:
Korekty artykułu:
-Języki publikacji:
AngielskiLiczba wyświetleń: 1917
Liczba pobrań: 1530